Ta.

Richard.
Moderators: slparry, Gromit, Paul
It'll be ok.............if you wear welding glovesstempy wrote:Hydroflouric acidSod that for a game of soldiers, I think I'll stick to me pot of elbow grease.
Purple AlertBoxadog 2000 wrote:Ok it is as follows and you use it at your own risk, it is a commercially available product from Chemetall (Schweiz) AG part of the Nobel group (and they make explosives).
Antox Stainless Steel Pickling Paste for the treatment of corrosion-and acidresistant stainless steels (which I am not sure that the beemer pipes are) the plastic container has all of the usual hazard warnings on ie skull and cross bones corrosive to hands ferrous steel etc etc.
Basically what it does is this, it removes all of the discoloration from stainless steel if you pipes are scabby it will not remove this but it will remove all of the dis-coloration ie brown/blue/straw colours.
You end up with Mat silver stainless steel which is very easy to then polish up to a chrome like finish.
Contains 6% hydroflouric acid and 20% nitric acid feck knows what the rest is
Works fine for me saves ages on polishing
This was my answer but it's still sat in the garage behind the bike with the scruffy headers. I'll give it a shot next spring.Archie wrote:Get a cheap bench grinder, £20, and a buffing wheel.Lightrunner wrote:Has anyone here tried Autosol?
You just have to take the headers off......